將磁精礦(-0.074mm粒級占6l%,-0.045mm粒級占54%)給入試驗室磨機進行磨礦,磨礦粒度分別為-0.045mm粒級占94.3%和99%,分別給入φ400mm×300mm鼓型濕式磁選機進行磁選試驗,給礦鐵品位為44.25%,磁場強度12.5kA/m,試驗指標見表5。由表5可以看出,磁精礦再磨至-0.045mm粒級占99%時,再次選別后品位達到56.48%,這與現(xiàn)場生產(chǎn)指標接近。 上一頁 [1] [2] [3] [4] [5] [6] [7] [8] [9] [10] [11] [12] [13] [14] [15] [16] [17] [18] [19] [20] [21] [22] [23] [24] [25] [26] [27] [28] [29] [30] [31] 下一頁 |