在400mL的燒杯中放入一定質(zhì)量的預(yù)處理凹凸棒土,然后加入鈦酸四丁酯與乙醇的混合溶液,用78一l型磁力加熱攪拌器攪拌同時(shí)用酸式滴定管滴加去離子水,控制去離子水加人體積(<3mL/min),攪拌時(shí)間為100min。然后用烘箱(